We are a prominent firm engaged in manufacturing, trading and exporting a wide range of Flexolet Threaded. We manufactured using top quality materials that are procured from reliable vendors in the market. These are developed under the strict supervision of our experts, who possess several years of experience in this domain. We provide these Flexolet Threaded to our clients at competitive prices.
ASTM B366 Inconel 625 Flexolet Threaded
Specifications
Standards |
Designation |
ASTM |
B 366 |
ASME |
SB 366 |
UNS |
N06625 |
Werkstoff Nr. |
2.4856 |
Dimensions
Chemical Composition
|
Inconel 625 |
Ni |
58.0 min |
Cr |
20.0 – 23.0 |
Fe |
5.0 max |
C |
0.10 max |
Mn |
0.50 max |
Si |
0.50 max |
Mo |
8.0 – 10.0 |
Co |
1.0 max |
Al |
0.40 max |
Ti |
0.40 max |
Nb + Ta |
3.15 – 4.15 |
P |
0.015 max |
S |
0.015 max |
Mechanical & Physical Properties – Inconel 625
Density |
8.4 g/cm3 |
Melting Point |
1350 °C (2460 °F) |
Tensile Strength |
Psi – 135,000 , MPa – 930 |
Yield Strength (0.2%Offset) |
Psi – 75,000 , MPa – 517 |
Elongation |
42.5 % |
Subcategory: Metal; Nickel Base; Superalloy
Key Words: ASME SB-443, SB-444, SB-446, SB-564, Boiler Code Sections I, III, VIII, IX; AFNOR NC 22 D Nb; VdTUV 499, AMS 5581, AMS 5599, AMS 5666, AMS 5837; DIN 17744, 17750-17752, 17754; Werkstoff Nr. 2.4856; NACE MR-01-75, UNS N06625; BS 3072, 3074, 3076 (NA21); ASTM B443, ASTM B444, ASTM B446, ASTM B564, ASTM B704, ASTM B705, ASTM B751
Component
Al
C
Co
Cr
Fe |
Wt. %
Max 0.4
Max 0.1
Max 1
20 - 23
Max 5 |
Component
Mn
Mo
Nb
Ni |
Wt. %
Max 0.5
8 - 10
3.15 - 4.15
Min 58 |
Electrical Properties |
Electrical Resistivity |
0.000129 ohm-cm |
0.000129 ohm-cm |
|
Magnetic Permeability |
1.0006 |
1.0006 |
at 200 oersted (15.9 kA/m) |
Curie Temperature |
Max -196 °C |
Max -321 °F |
|
Thermal Properties |
CTE, linear 20°C |
12.8 µm/m-°C |
7.11 µin/in-°F |
20-100°C |
Heat Capacity |
0.41 J/g-°C |
0.098 BTU/lb-°F |
|
Thermal Conductivity |
9.8 W/m-K |
68 BTU-in/hr-ft²-°F |
|
Melting Point |
1290 - 1350 °C |
2350 - 2460 °F |
|
Solidus |
1290 °C |
2350 °F |
|
Liquidus |
1350 °C |
2460 °F |
|
Main Export Market
- Eastern Europe
- North America
- Mid East/Africa
- Central/South America
- Asia
- Western Europe
- Australasia
- UAE
Sales Locations
U.A.E,
Oman,
Saudi Arabia,
Qatar,
Bahrain,
Egypt,
Turkey
Singapore,
Thailand,
Malaysia
Indonesia
Poland
Italy
Portugal
Spain
Brazil
Chile
Venezuela
Costa Rica
USA
Canada
Angola
Sri Lanka
Russia